I have used Penetrox on all of my element sections for the last 15 years.
Prior to that I used nothing and occasionally had issues removing the
pieces. If you're in a corrosive environment I would definitely recommend
using it unless something is different about Tennadyne construction compared
to normal yagi elements. I seem to recall Telrex having similar warnings
which is maybe why my early yagis were assembled dry.
John KK9A
To: <towertalk@contesting.com>
Subject: [TowerTalk] Tennadyne Element installation
From: "James Wolf" <jbwolf@comcast.net>
Reply-to: jbwolf@comcast.net
Date: Fri, 1 Jul 2016 17:47:28 -0400
I obtained a used Tennadyne Model T8 for my short tower and am getting ready
to put it back together.
The instructions state that I should not use ANTI-OXIDE grease; in bold
letters. Instead they recommend using WD-40 or graphite.
I've always used it for assembling antenna elements. Is there any good
reason to not use ANTI-OXIDE inside the element extensions?
Jim - KR9U