It will not take much power to get way more then 1A through a piece of
copper wire in a RF tuned system.
>From my experience, soft soldered connections won´t last long when outside
and when the solder joint is not weather proof protected.

73
Peter



Jim Miller KG0KP wrote:

> Now we mix Tin(60)/Lead(40) and get 10.6 microhms per centimeter.  Now 
> the distance we are talking about is NOT 1 cm.  Not even one mm but
> lets use that anyway ( more like 0 to 1/10 mm).   So, we have 1.06 
> microhms.  Now it will take approximately 1,000,000 volts to get an 
> amp at that point. 

_______________________________________________



_______________________________________________
TowerTalk mailing list
TowerTalk@contesting.com
http://lists.contesting.com/mailman/listinfo/towertalk

<Prev in Thread] Current Thread [Next in Thread>