| To: | "Larry Benko" <xxw0qe@comcast.net>, <amps@contesting.com> |
|---|---|
| Subject: | Re: [Amps] Skin depth: silver plating of tank circuit coil feasible with chemical plating kits? |
| From: | "David Cutter" <d.cutter@ntlworld.com> |
| Date: | Mon, 4 Oct 2010 17:36:05 +0100 |
| List-post: | <amps@contesting.com">mailto:amps@contesting.com> |
Great set of tests Larry. Here is some stuff from the old days which I've posted here a few times: http://www.k6mhe.com/n7ws/Plating.pdf and http://www.k6mhe.com/n7ws/Fowler_Errata.pdf David G3UNA > Take a look at http://www.bnk.com/w0qe/inductor_Q_tests.html where I > made a bunch of measurements. > > Silver is a 7% better conductor than copper but at RF the skin depth is > inversely proportional to the conductivity so the gain you get from > heavy silver plating is only about 3.5% to 4%. You would be better off > to just increase the copper wire size by 1. As far as beauty is > concerned, painting or clear coating the copper has no effect at HF. > All the stuff you hear about oxides of silver being conductors are BS. > > Larry, W0QE _______________________________________________ Amps mailing list Amps@contesting.com http://lists.contesting.com/mailman/listinfo/amps |
| <Prev in Thread] | Current Thread | [Next in Thread> |
|---|---|---|
| ||
| Previous by Date: | Re: [Amps] Skin depth: silver plating of tank circuit coil feasible with chemical plating kits?, Larry Benko |
|---|---|
| Next by Date: | Re: [Amps] Skin depth: silver plating of tank circuit coil feasiblewith chemical plating kits?, Carl |
| Previous by Thread: | Re: [Amps] Skin depth: silver plating of tank circuit coil feasible with chemical plating kits?, Larry Benko |
| Next by Thread: | Re: [Amps] Skin depth: silver plating of tank circuit coil feasiblewith chemical plating kits?, Carl |
| Indexes: | [Date] [Thread] [Top] [All Lists] |