I was at Ten-Tec once and they showed me where they did that "potting." 
Dunno which ones they potted, though.

Mike N4NT

----- Original Message ----- 
From: "Lyle Dunlap" <lyle3dd@grics.net>
To: "Discussion of Ten-Tec Equipment" <tentec@contesting.com>
Sent: Monday, October 03, 2005 4:34 PM
Subject: Re: [TenTec] Reducing hum on Ten Tec 255 supply


Hi Steve,

What I would do being one who now and then winds xformers.  Dip it in
electrical varnish, pull vacuum on it and then bake it.  Probably a lot of
work if your not set up for it.  Probably some lazy ways of getting around
it but that would be the proper way.  Too bad xformer mfgrs do not do that
in the first place.
Know ur getting other advice, anyway lots a luck 73
Lyle W9FCX 
_______________________________________________
TenTec mailing list
TenTec@contesting.com
http://lists.contesting.com/mailman/listinfo/tentec

<Prev in Thread] Current Thread [Next in Thread>