I live in a salt-air environment and have replaced just about all U-bolts and other such hardware with stainless steel. Be sure to coat bolts with an appropriate compound before installing nuts--if you are not familiar with this, ask your SS supplier. Also, per advice from F12 many years ago, I assembled elements and then painted them with XIM400, which has protected them nicely. At some points, I have had over 50 F12 elements up at the edge of a cliff with saltwater to the horizon and little fluffy balls of salty foam flying up and over. 73, Jim, VE1JF _______________________________________________ _______________________________________________ TowerTalk mailing list TowerTalk@contesting.com http://lists.contesting.com/mailman/listinfo/towertalk |
<Prev in Thread] | Current Thread | [Next in Thread> |
---|---|---|
|
Previous by Date: | Re: [TowerTalk] Force 12 Hardware Question, Bryan Swadener |
---|---|
Next by Date: | Re: [TowerTalk] Force 12 hardware and aluminum treatment for corrosion resistance, john |
Previous by Thread: | [TowerTalk] Force 12 Hardware Question, Gerard Jendraszkiewicz |
Next by Thread: | Re: [TowerTalk] Force 12 hardware and aluminum treatment for corrosion resistance, john |
Indexes: | [Date] [Thread] [Top] [All Lists] |