summing all the cost involving  Regalvanizing  several
Towers pieces , i read cost for the work to do it,
plus if your tower is UP, removing all the sections,
transport to the company , all this cost and later the
cost to put all again , i think  for some will be
cheaper and faster  buy new sections or used in better
conditions  and sell the rust ones to others that want
to  pay the "cheap tower" and the regalvanizing work

i think will be good a final cost analysis to know  if
pay  or not to perform all the work, maybe for a R25g
will not pay (unless free and at groun level), for
bigger tower can be an option if the tower was buyed
cheap and is at the ground.

others  just "repair" the rust with cold galvanizing 
or just swap the section.


other think, the paint used in comercial towers is
Water Based Latex Emulsion   under the name of Blended
Vinyl Acrylic Emulsion , rohn-radian sell it   with
this use:

Water Based Tower Paint for use on untreated
galvanized surfaces. Vinyl/acrylic emulsion resin
provides long-term protection and performance. Offers
resistance to weather, ease of application with a
paint mitt, and freedom from fire hazard. Meets FAA
regulations for color-coding. 

Hector G

--- GALE STEWARD <k3nd@yahoo.com> wrote:

> Another "minor" issue is that a tower can be painted
> in place. Regalvanizing is fine if all the sections
> are apart and on the ground.
> 
> K3ND
> 
> 
> 
> --- Jim Jarvis <jimjarvis@verizon.net> wrote:
> 
> > 
> > The answer to "why not 'just' regalvanize?" lies
> > with the distance to the galvanizing outfit, and 
> > the galvanizing cost, plus the condition of the
> > tower.  
> > 
> > It's not cheap to do, particularly if you have to 
> > truck the load several hundred miles each way.
> > 
> > In addition, most galvanizers won't touch a rusted
> > structure.  You can't zinc plate over iron oxide.
> > So if you see internal rust, it's probably a lost
> > cause.
> > 
> > n2ea
> > 
> > _______________________________________________
> > 
> > 
> > 
> > _______________________________________________
> > TowerTalk mailing list
> > TowerTalk@contesting.com
> >
>
http://lists.contesting.com/mailman/listinfo/towertalk
> > 
> 
> 
> __________________________________________________
> Do You Yahoo!?
> Tired of spam?  Yahoo! Mail has the best spam
> protection around 
> http://mail.yahoo.com 
> _______________________________________________
> 
> 
> 
> _______________________________________________
> TowerTalk mailing list
> TowerTalk@contesting.com
>
http://lists.contesting.com/mailman/listinfo/towertalk
> 


Hector Garcia XE2K / XF1K
Mexicali B.C  DM22fp

http://www.dxxe.org
_______________________________________________



_______________________________________________
TowerTalk mailing list
TowerTalk@contesting.com
http://lists.contesting.com/mailman/listinfo/towertalk

<Prev in Thread] Current Thread [Next in Thread>