In a message dated 99-07-21 12:19:49 EDT, K7NV@contesting.com writes:

> ASTM A 475 lists 3/8 EHS at 15400 Lb min breaking strength.
>  So if you are trying to get a strength equivalent look for HPTG 15400
>  Phillystran. 
>  They also make 20800, 27000, 35000, 42400, 58300....up to 160000

    Kurt is right as usual. The original question was in regard to 25G. 3/8" 
EHS is NOT a factory specified material for Rohn 25G. Use of 3/8" EHS with it 
should be done with caution and is a violation of the LXC Prime Directive of 
"DO what the manufacturer says". 

Cheers,  Steve    K7LXC

--
FAQ on WWW:               http://www.contesting.com/towertalkfaq.html
Submissions:              towertalk@contesting.com
Administrative requests:  towertalk-REQUEST@contesting.com
Problems:                 owner-towertalk@contesting.com
Search:                   http://www.contesting.com/km9p/search.htm


<Prev in Thread] Current Thread [Next in Thread>