| Roger L. Elowitz wrote:
> 
>
> And... for you chemists (or alchemists)... what is it about a eutectic
> solder that makes it any different than ordinary flux-cored 60/40?
> Enquiring minds want to know?
> 
> Roger, K2JAS
> 
Only refers to the melting point, usually around 400 degrees F.
I don't think it makes a good penetration into the material that's
being worked on, but - then I'm guessing. de KL7HF
--