Scott,

Any reputable supplier of specialty steels, such as 4130, will
routinely provide you with the metalurgical test results for the steel
tubing you have purchased. Some suppliers charge a few dollars for the
test certificate.

I wouldn't use a specialty steel without having the test document,
otherwise there is no way to have confidence in your installation!

73
Frank
W3LPL
donovanf@sgate.com

> ---------------------
> Forwarded message:
> From: KB3X@msn.com (Scott Hudler)
> I do have a question or two.  I have determined that with my three antennas I
> 
> will need a mast capable of 65000 PSI Y.S.  It also recommends .250" wall 
> thickness.  Will it matter what the wall thickness is as long as the Y.S. is 
> at least the desired value?  The supplier I found claims that his 4130 .250" 
> wall is rated at 100,000 PSI or better and that I probably could go with
> .188"  or .156" wall instead.  Any thoughts?  


--
FAQ on WWW:               http://www.contesting.com/towertalkfaq.html
Submissions:              towertalk@contesting.com
Administrative requests:  towertalk-REQUEST@contesting.com
Problems:                 owner-towertalk@contesting.com

<Prev in Thread] Current Thread [Next in Thread>