Search String: Display: Description: Sort:

Results:

References: [ +subject:/^(?:^\s*(re|sv|fwd|fw)[\[\]\d]*[:>-]+\s*)*\[TowerTalk\]\s+Galvanizing\s+4130\?\s*$/: 2 ]

Total 2 documents matching your query.

1. [TowerTalk] Galvanizing 4130? (score: 1)
Author: w8mm@ibm.net (Mike Valentine - W8MM)
Date: Thu, 23 Oct 1997 21:50:42 +0100
Hi all! I have a "normalized" 4130 2"O.D. mast that I think I want to galvanize. It has a black colored outside surface condition as supplied from the metal dealer. I am wondering if there are any tr
/archives//html/Towertalk/1997-10/msg00660.html (7,294 bytes)

2. [TowerTalk] Galvanizing 4130? (score: 1)
Author: twoway@scoden.ma.ultranet.com (Scott Bullock)
Date: Thu, 23 Oct 1997 19:02:00 -0400
Mike, I just put up a 24' piece of this, it was also black and covered with oil when it was picked up. I had spoken to a galvanizing shop about this, they had no problem doing it, they pickle it then
/archives//html/Towertalk/1997-10/msg00662.html (8,868 bytes)


This search system is powered by Namazu