21. Re: [TowerTalk] Experience with Sacrificial Zinc? (score: 1)
Author: M?ximo EA1DDO_HK1H <ea1ddo@hotmail.com>
Date: Tue, 10 Aug 2021 17:25:47 +0000
I can see Rust-Oleum sells Urethane Aliphatic enamel: https://www.rustoleum.com/product-catalog/industrial-brands/commercial/urethane-coatings/3300-system-acrylic-aliphatic-urethane-coating 73, Maxim
/archives//html/Towertalk/2021-08/msg00054.html (11,739 bytes)

22. Re: [TowerTalk] Experience with Sacrificial Zinc? (score: 1)
Author: <john@kk9a.com>
Date: Tue, 10 Aug 2021 17:50:34 -0400
I have had very good luck with Brite Zinc cold galvanizing paint in normal environments (i.e. not the ABC islands). Even galvanizers use cold galvanizing paint to touch up missed areas. I do not beli
/archives//html/Towertalk/2021-08/msg00055.html (8,922 bytes)

23. Re: [TowerTalk] Experience with Sacrificial Zinc? (score: 1)
Author: Grant Saviers <grants2@pacbell.net>
Date: Tue, 10 Aug 2021 17:51:40 -0700
Rich, Galvanizing is so local (~1/4") for protecting bare/rusting steel that I don't think a zinc will help. Since the PJ4 rust is apparently well developed there are some conversion + paint coatings
/archives//html/Towertalk/2021-08/msg00061.html (12,882 bytes)

24. Re: [TowerTalk] Experience with Sacrificial Zinc? (score: 1)
Author: Richard Smith <n6kt1@sbcglobal.net>
Date: Wed, 11 Aug 2021 01:28:58 +0000 (UTC)
Hi John, On Aruba, did you have any trouble having the Brite Zinc adhere to various HDG parts? We have been using Brite Zinc as well on Bonaire, and it seems to adhere to some parts very well, but fl
/archives//html/Towertalk/2021-08/msg00065.html (10,212 bytes)

25. Re: [TowerTalk] Experience with Sacrificial Zinc? (score: 1)
Author: <n0tt1@juno.com>
Date: Wed, 11 Aug 2021 16:58:39 +0000
I wouldn't think a primer would allow the zinc overcoating to adhear to the base metal. Right? Charlie, N0TT _______________________________________________ _________________________________________
/archives//html/Towertalk/2021-08/msg00072.html (10,000 bytes)